A circular iron bangle, made from a rounded iron rod with abutting ends (bottom of photo). The bangle's surface is corroded by rust. This artifact was found closely associated with a copper alloy twinned figurine, a tanged iron blade, a rounded quartz pebble and several other objects, which archaeologists interpret as a shrine cluster. The cluster was placed among metal-working features in a metallurgical workshop.Scale in cm. Maximum diameter: 8.1 cm. Weight: 75 g. Site Ngre Kataa. 19 July 2008.
Triangular-headed iron projectile point with a barb at the head's base (left) and a long tang (right). To make an arrow (snini in Nafaanra), the tang was inserted into a straight shaft made of bamboo, reed or lightweight wood to which it was hafted. This artifact was found in an area (mound 7) that archaeologists interpret as a house mound. The projectile point shows signs of corrosion by rusting. Scale in cm. Length: 9 cm. Weight: 9.2 g. Site Ngre Kataa. 7 July, 2008.
Triangular-headed iron projectile point (SF 09-033) with a slightly squared base (left ) and a short tang (right). To make an arrow (snini in Nafaanra), the tang was inserted into a straight shaft made of bamboo, reed or lightweight wood to which it was hafted. This artifact was found close to several anvil/grinding stones in an area (mound 6) that archaeologists interpret as a metallurgical workshop. The projectile point shows signs of corrosion by rusting. Scale in cm. Length: 8.1 cm. Weight: 9.3 g. Site Ngre Kataa. 30 May 2009.
Iron projectile point with an asymmetrical head (left), a single barbed at the base of the head and a small barb on the opposite side along the tang. To make an arrow, the long tang (right) would have been inserted into a shaft made of bamboo, reed or lightweight wood. This artifact was found in an area (mound 6) that archaeologists interpret as a metallurgical workshop. The point has been corroded by rusting. Scale in cm. Length: 15.2 cm. Weight: 13.7 g. Site Ngre Kataa. 2 June 2009.
Triangular-headed iron projectile point with a single barb at the base of its head (left) and a long thin tang (right). To make an arrow (snini in Nafaanra), the tang was inserted into a shaft made of bamboo, reed or lightweight wood to which it was hafted. The artifact shows signs of corrosion. The point was excavated from a deep midden mound in an disturbed by a pig burrow. Scale in cm. Length: 12.4 cm. Weight: 14.2 g. Site Ngre Kataa. 25 June, 2008.
Triangular-headed projectile point with barbs on either side of the head's base (left). Its long tang (right) is bent. To make an arrow (snini in Nafaanra), the tang was inserted into a straight shaft made of bamboo, reed or lightweight wood to which it was hafted. This artifact was found in an area that archaeologists interpret as a metallurgical workshop. The projectile point shows signs of corrosion by rusting. Scale in cm. Length: 9.8 cm. Weight: 10.2 g. Site Ngre Kataa. 5 July, 2008.
Rights:
Creative Commons Attribution-NonCommercial
Publisher:
University of Victoria Libraries
Provenance:
Ngre Kataa, Mound 6, Unit 44N 6W, Level 3; piece plot: 67-71 cm S, 142-156 W
A flat, thin iron disk. The object is corroded by rust. Its function is unknown. The disc was found in close association with a large anvil or grinding stone and adjacent to a distinctive pottery vessel and a smaller, irregularly shaped piece of flat iron (SF 09-171). This group of objects was located within an area (mound 6) that archaeologists interpret as a metallurgical workshop. Scale in cm. Width: 9.4 cm. Thickness: .2 cm. Weight: 49.3 g. Site Ngre Kataa. 4 July 2009.
A flat, irregularly shaped iron with circular depression. The object is corroded by rust and its original form and function are unknown. It was found in close association with a large anvil or grinding stone (GS 09-15), a circular iron disk (SF 09-370) and a distinctive pottery vessel (NK 09-787). This group of objects was located within an area (mound 6) that archaeologists interpret as a metallurgical workshop. Scale in cm. Width: 5.7 cm. Thickness: .2 cm. Weight: 9 g. Site Ngre Kataa. 4 July 2009.
Partial iron projectile point, the tip of the head (left) broken off. The base of the head forms a right angle barb with the short tang. The tang (right) would have been inserted into a shaft made of bamboo, reed or lightweight wood to form an arrow. This point was found in an area (mound 7) that archaeologists interpret as a house mound. The artifact is corroded by rust. Scale in cm. Length: 9.1 cm. Weight: 13.6 g. Site Ngre Kataa. 4 June 2009.
Flat, thin iron disk (SF 09-159). The object is corroded by rust and its edges notched in two spots. Its function is unknown. The disc was found in a cluster (cluster D) with an iron bangle (SF 09-158) and two stones whose surfaces showed evidence of grinding. The cluster was part of a wider feature (clusters A-D) that archaeologists interpret as a shrine, which overlaid stratified deposits in a metallurgical workshop (mound 6). Scale in cm. Width: 8.1 cm. Thickness: .2 cm. Weight: 29.8 g. Site Ngre Kataa. 9 June 2009.